C and Z purlins are cold formed sections: a flat steel strip is rolled into shape at room temperature, not hot rolled like an angle or channel. The C has a web, two flanges and two small lips that stiffen the flange edges. The Z has the same parts, but the flanges point in opposite directions.
They are made from thin steel, usually about 1.6 mm to 3.15 mm thick, in depths of about 100 mm to 300 mm. For sheds the most common depths are 150 mm and 200 mm. Many are made from pre-galvanised high strength coil, so they come rust protected from the factory. Black (uncoated) ones need painting.
- Size is written as depth x flange x lip x thickness, for example C 200 x 75 x 20 x 2.0 mm.
- Depth decides how far the purlin can span. Thickness decides how much load it can take at that span.
- Design of cold formed light gauge sections in India follows IS 801. Leave the design to an engineer.
Why Z purlins are lapped
A Z section can nest inside another Z of the same size. So at each rafter, the end of one Z purlin overlaps the start of the next and the two are bolted together. This lap makes the purlins act like one continuous beam over several rafters instead of a chain of separate short beams.
A continuous purlin bends less and carries more load for the same weight, which is why Z purlins are the usual choice in pre-engineered buildings with long bays. The lap length and bolt pattern are set by the designer, so follow the drawing exactly. C purlins cannot nest, so they are usually used as simple spans, butted or sleeved at the supports.
MS angle, SHS and RHS purlins
An MS angle (for example ISA 65 x 65 x 6 or 75 x 75 x 6) is hot rolled, thick and easy to weld. Every welder in a small town can work with it, and J hooks fit around it neatly. The trouble is that an angle is not deep, so it is not very stiff in bending for its weight. It suits short purlin spans.
SHS and RHS (square and rectangular hollow sections, often called pipe purlins) are stiffer than angles of similar weight, look neat, are easy to paint on the outside, and take self-drilling screws well. An RHS such as 96 x 48 x 3.2 mm or 80 x 40 x 3.2 mm is a common purlin on small and medium sheds. The inside cannot be painted, so seal the ends to keep moisture out.
Weight and stiffness compared
The table gives approximate weights per metre for some common purlin sections. Weights are worked out from steel density and can vary slightly by maker. The point to notice is that a 200 mm deep C weighs about the same as a 75 mm angle, but because it is nearly three times deeper it is many times stiffer in bending.
| Section | Approx. kg per metre | Typical use |
|---|---|---|
| ISA 65 x 65 x 6 angle | 5.8 | Small sheds, short purlin spans |
| ISA 75 x 75 x 6 angle | 6.8 | Farm and shop sheds, short spans |
| RHS 80 x 40 x 3.2 | 5.5 to 5.7 | Small to medium sheds |
| RHS 96 x 48 x 3.2 | 6.7 to 6.9 | Medium sheds, neat finish |
| C 150 x 65 x 20 x 2.0 | 4.9 to 5.0 | Medium bays, factory sheds |
| C 200 x 75 x 20 x 2.0 | 6.0 to 6.1 | Longer bays, PEB style sheds |
| C or Z 200 x 75 x 20 x 2.5 | 7.5 to 7.6 | Long bays, higher wind or loads |
Use our weight charts for angles and pipes to total the steel for your shed. For C and Z purlins, ask the maker for their section table.
Which one fits your shed
- Small farm, dairy or shop shed with trusses or rafters 3 to 4 m apart: MS angle or RHS purlins are simple, easy to source and easy to weld. Most local fabricators prefer them.
- Medium shed with frames 5 to 6 m apart: RHS or C purlins. Deeper sections are needed as the gap between frames grows.
- Large span factory or warehouse with frames 6 m or more apart: C or lapped Z purlins, usually designed with the PEB frame.
- Very corrosive places (cattle sheds, fertiliser or chemical stores): choose galvanised purlins or give black steel a good primer and paint system, and keep up maintenance.
- Whatever you choose, get the frame designed by an engineer. Purlin size depends on span, sheet weight, wind and slope, not on habit.
Fixing and site care for C and Z purlins
- Thin sections are weak sideways. Sag rods or bridging at mid span or third points keep them straight; do not skip them.
- Bolt C and Z purlins to cleats on the rafter. Avoid heavy site welding on galvanised thin sections, it burns the coating and can distort the steel.
- Follow the drawing for which way the open side of a C faces. It usually faces up the slope.
- Use self-drilling screws with a drill point matched to the purlin thickness.
- Do not stand or walk on the lip edge during erection; thin lips dent easily.
Frequently asked questions
- Is a C purlin stronger than an MS angle?
- For the same weight per metre, a C purlin is much stiffer in bending because it is deeper. An angle is thicker and more forgiving of rough handling and welding. Which is right depends on the span and how the shed is built.
- What thickness of C purlin is used for sheds?
- Common thicknesses are about 1.6 mm to 3.15 mm. Small and medium sheds often use 2.0 to 2.5 mm, but the right thickness comes from the design for your span and wind load.
- Why are Z purlins overlapped at the rafters?
- The lap makes the purlins act as one continuous beam over several frames, which reduces bending and saves steel. The lap length and bolts must follow the designer's drawing.
- Can I weld C purlins?
- Light welding of cleats is possible on black sections, but galvanised thin C and Z purlins are normally bolted. Welding burns off the zinc and can warp the thin steel. Touch up any welded spots with zinc rich paint.
- Do you supply purlins?
- We stock MS angles, channels and hollow sections, and can arrange C purlins on order. WhatsApp or call us with sizes and lengths for today's rate.